For the clear part, I'm using Smooth-On's EpoxAcast 690. I'm pressurizing that step of the process to 40-45 PSI. I haven't tried warming it (I'll give that a go), but I have let it sit. I'm not using a mold for the doming, I'm doing it by hand. The only part of the eye that is made using a mold is the sclera.